関西ペイント

エポマリン EX300

Product names, manufacturer names and thinner product names are kept in Japanese so you can match them with the can label at the store or on site.

Basic Information

Manufacturer関西ペイント
Use / Type
Use: Interior | Resin: Epoxy
Original (JA): 変性エポキシ樹脂塗料 箱桁内面用ポリアミド硬化変性エポキシ樹脂塗料(2液形)
Water-based / Solvent-basedStrong solvent-based, 2-component (aromatic-type)
1K / 2K2-component (2K)

Application Specifications

Dilution0–10%
Thinner / DiluentテクトEP内面用シンナー (thinner for tank-interior use)
Number of Coats1 coat(s)
Coverage (consumption)
airless: 450 g/m²
Brush / Roller: 240 g/m²
Recoat Time (drying interval)
5°C: Min 24 hours / Max 1 months
Usable time 10 hours
10°C: Min 24 hours / Max 1 months
Usable time 8 hours
20°C: Min 16 hours / Max 1 months
Usable time 6 hours
30°C: Min 12 hours / Max 1 months
Usable time 4 hours
40°C: Min 8 hours / Max 1 months
Usable time 2 hours
Mixing RatioBase 9:Hardener (Comp. B) 1
Pot Life10 hours (5°C) , 8 hours (10°C) , 6 hours (20°C) , 4 hours (30°C) , 2 hours (40°C)
Induction time (after mixing)30 minutes
Field Notes (JA)・ 箱桁内面用。
・ 浮きさび・ルーズな黒皮・旧塗膜の発錆等は十分除去して塗装する。
・ 標準膜厚60µm/回。

* For heavy-duty anticorrosion work, the number of coats and the film thickness are fixed by the painting specification of each project. The figures shown here are the maker's standard values.

⚠️ Cautions & Notes (Japanese original)

To avoid mistranslation of safety-critical information, the notes below are kept in the original Japanese. Please check them with a translation app, or ask a Japanese-speaking colleague. Always follow the official manufacturer TDS.

⚠️ Please verify before use
The values above are reference values based on the manufacturer's official catalogs and technical data sheets (TDS). Specifications may change. Always check the product label and the latest official TDS before actual application.